Chemical composition: Chemical Composition C Si Mn P S Ni Cr Cu ≤ 60 0.57 to 0.65 0.17 to 0.37 0.50 to 0.80 0.30 0.25 0.25 0.035 0.035 65 0.62 to 0.70 0.17 to 0.37 0.50 to 0.80 0.30 0.25 0.25 0.035 0.035
Mechanical properties: Grades blank sample Size / mm heat treatment process of the mechanical properties of the steel hardness delivery status / HBS Normalizing quenching and tempering σb / MPa σs / MPa δ5 (%) ψ (%) Ak / J ≤ ≥ No heat annealed steel 60 25 8,106,754,001,235,255,229 65 25 8,106,954,101,030,255,229
Characteristics and Uses: 60 steel strength, hardness and elasticity are quite high, but when the cold plastic deformation is low, poor machinability, weldability and hardenability is poor, water quenching cracks tend to have only small parts can be quenched, large multi-normalizing for the manufacture of rollers, shafts, eccentric shafts, spring rings, cam, spring washers, clutch, rope and other larger force, working under the friction conditions, requiring high strength, wear resistance and elasticity of certain parts 65 steel, for the manufacture of springs, coil springs, various gaskets, clutches and shaft manufacturing general machinery, roller, eccentric shaft. |