Japan SKD11 in datong DC53 steel based on improved, hardness higher SKD11, High temperature (520-53 ° c) after tempering can reach high hardness, 63HRC 62 - more than SKD11 in intensity. 2 and toughness is SKD11 twice. DC53 toughness in the cold die in, Therefore, the use of DC53 cracks, and few can greatly improve the service life. 3, wire-cutting processing of residual stress, high-temperature tempering reduced residual stress. Therefore, the large moulds and requirements of precision mould in wire-cutting plus |